Precision Machined Steel Components with Ra 0.4um Sealing Faces and Electroless Nickel Plating for Quench and Temper 28-32 HRC Transmission Parts

Precision Machined Steel Components with Ra 0.4um Sealing Faces and Electroless Nickel Plating for Quench and Temper 28-32 HRC Transmission Parts
Basic Properties
Country Of Origin
Guangdong, China
Brand Name
Leshine
Certificate
ISO 9001:2015
PRODUCT MODEL
ST-FIN-42CR
Trading Properties
MOQ
1 Piece
Unit Price
USD 9.9-380 / Piece
Payment Method
T/T,L/C,PayPal,Western Union
Supply Capacity
50000 Pieces per Month
Product Summary

42CrMo4 steel components machined to Ra 0.4um on sealing faces with electroless nickel plating, heat treated and inspected with roughness and coating reports.

Product Details
Highlight:

Steel Components Surface Finish Ra 0.4

,

Electroless Nickel Plated Steel Parts

,

42CrMo4 Precision Turned Components

Materials: 42CrMo4 / SCM440, 20CrMnTi, C45, 4140, 17-4PH
Heat Treatment: Quench And Temper 28-32 HRC, Carburizing, Induction Hardening
Surface Finish: Ra 0.4um Sealing Faces, Ra 0.8um Bearing Seats, Ra 1.6um General
Finish Options: Electroless Nickel 8-12um, Black Oxide, Hard Chrome, Zinc Nickel, Phosphate
Tolerance: +/-0.01mm General, +/-0.005mm On Ground Features
Processes: CNC Turning, Milling, Cylindrical Grinding, Honing, EDM
Inspection: CMM, Roughness Tester, Hardness Tester, Coating Thickness Gauge
Documentation: Material Certificate 3.1, Heat Treatment And Plating Reports
Product Description
Steel Components with Controlled Surface Finish

42CrMo4 / SCM440  •  Surface Finish Ra 0.4–1.6 µm  •  Electroless Nickel and Black Oxide

Components are turned and milled from 42CrMo4 bar, heat treated to the drawing hardness, and then finished to the surface roughness called out per face rather than across the whole part. Sealing faces and bearing journals are brought down to Ra 0.4 µm, non-functional faces stay at Ra 1.6 µm, and the electroless nickel or black oxide layer is applied after a stress relief so the coating does not craze in service.

  • Ra 0.4 µm on sealing faces and journals, Ra 1.6 µm elsewhere, measured per face
  • Electroless nickel 8–12 µm with coating thickness and adhesion checks
  • Hardness and case depth confirmed before finishing, not after the batch
Finish Is Part of the Machining Plan, Not a Last Step
Grind Where Turning Cannot Reach Ra 0.4

Hardened steel above 45 HRC is ground or honed after heat treatment, because a turning insert will not hold the surface once the material work hardens.

Coating Thickness Allowed In

Electroless nickel adds 8–12 µm per surface. Threads, bores, and fits are machined undersize by that amount, so the plated part still gauges inside the drawing.

No Hydrogen Embrittlement Surprises

Plated high-strength parts are baked within the required window after coating, which is what keeps a hardened transmission component from cracking under load.

Roughness Reported Per Face

A roughness trace is recorded on the sealing faces and journals and shipped with the dimensional report, so the value you receive is measured rather than assumed.

Steel Component Specifications
Parameter Specification
Materials 42CrMo4 / SCM440, 20CrMnTi, C45, 4140, 17-4PH, 316L on request
Heat Treatment Quench and temper 28–32 HRC, carburizing, induction hardening, stress relief
Surface Finish Ra 0.4 µm on sealing faces and journals, Ra 0.8 µm bearing seats, Ra 1.6 µm general faces
Finish Options Electroless nickel 8–12 µm, black oxide, hard chrome, zinc nickel, phosphate, DLC on request
Tolerances ±0.01 mm general, ±0.005 mm on ground features, per drawing and GD&T
Processes CNC turning, milling, drilling, tapping, cylindrical grinding, honing, EDM
Diameter Range 5 mm to 300 mm turned, up to 800 mm length
Inspection CMM, roughness tester, hardness tester, coating thickness gauge, thread gauges
Documentation Material certificate 3.1, heat treatment report, plating thickness report, dimensional and roughness report
Drawing Formats STEP, IGES, X_T, SolidWorks, DWG, PDF with GD&T
Production Volume Prototype 1–100 pcs, low volume 101–10,000 pcs, high volume above 10,001 pcs
Order Route for Finished Steel Components
  1. Drawing review confirms which faces carry a roughness callout, which need grinding, and how much coating allowance to leave.
  2. Rough machining, then heat treatment to the specified hardness with the test bar from the same lot.
  3. Finish turning and grinding to size, with roughness measured on the sealing faces before the part leaves the machine.
  4. Cleaning, masking, and coating, then baking where the hardness requires it and re-check on threads and bores.
  5. Final inspection, oiled and VCI packed with the plating, hardness, and roughness reports inside the carton.
Where These Components Are Used

Transmission shafts and gear seats, hydraulic cylinder rods and pistons, valve stems and spools, pump drive components, spindle and arbor parts, die and mold inserts, clamping and fixture components, and general machinery parts that need a defined sealing face. The same finishing logic applies to a single replacement part and to a production batch, because roughness and coating allowance are written into the process routing rather than added at the end.

Send Your Drawing With Finish Callouts